  4. Temperature dependence of the PER in PM PCF coil

Temperature dependence of the PER in PM PCF coil

上传者: 2021-02-21 18:26:33上传 PDF文件 243KB 热度 21次
A piece of domestic polarization-maintaining photonic crystal fiber (PM-PCF, 964 m in length) is made into a fiber coil, and its polarization extinction ratio (PER) is measured in a temperature range of –45–80 oC before and after PM-PCF is wound and solidified. A fiber coil made of commercial panda